| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 88.0 MPa @Temperature 23.0 °C |
12800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | 16 % @Temperature 23.0 °C |
16 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| Elongation at Yield | 4.6 % @Temperature 23.0 °C |
4.6 % @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Modulus | 3.05 GPa @Temperature 23.0 °C |
442 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Charpy Impact Unnotched | 13.4 J/cm² @Temperature -30.0 °C |
63.8 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
| 20.3 J/cm² @Temperature 23.0 °C |
96.6 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 0.370 J/cm² @Temperature -30.0 °C |
1.76 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
| 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | DAM; ISO 75-1/-2 |
| UL RTI, Electrical | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
DAM; UL 746B |
| 65.0 °C @Thickness 6.00 mm |
149 °F @Thickness 0.236 in |
DAM; UL 746B | |
| 130 °C @Thickness 0.710 mm |
266 °F @Thickness 0.0280 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
DAM; UL 746B |
| 65.0 °C @Thickness 6.00 mm |
149 °F @Thickness 0.236 in |
DAM; UL 746B | |
| 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 65.0 °C @Thickness 0.400 mm |
149 °F @Thickness 0.0157 in |
DAM; UL 746B |
| 65.0 °C @Thickness 6.00 mm |
149 °F @Thickness 0.236 in |
DAM; UL 746B | |
| 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
DAM; UL 746B | |
| Flammability, UL94 | V-2 @Thickness 6.00 mm |
V-2 @Thickness 0.236 in |
DAM; IEC 60695-11-10 |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 6.00 mm |
V-2 @Thickness 0.236 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 0.710 mm |
V-2 @Thickness 0.0280 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; UL94 | |
| V-2 @Thickness 0.710 mm |
V-2 @Thickness 0.0280 in |
DAM; UL94 | |
| V-2 @Thickness 0.400 mm |
V-2 @Thickness 0.0157 in |
DAM; UL94 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; UL94 | |
| V-2 @Thickness 0.400 mm |
V-2 @Thickness 0.0157 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 6.00 mm |
V-2 @Thickness 0.236 in |
DAM; UL94 | |
| V-2 @Thickness 6.00 mm |
V-2 @Thickness 0.236 in |
DAM; UL94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; UL94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; UL94 | |
| Glow Wire Test | 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 |
| 750 °C @Thickness 1.50 mm |
1380 °F @Thickness 0.0591 in |
DAM; Ignition; IEC 60695-2-13 | |
| 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
DAM; IEC 60695-2-12 | |
| 960 °C @Thickness 0.710 mm |
1760 °F @Thickness 0.0280 in |
DAM; IEC 60695-2-12 | |
| 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
DAM; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
| 280 - 300 °C | 536 - 572 °F | DAM | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; optimum |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA66< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Unreinforced Resins | DAM |
| Resin Identification | PA66 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |