| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
| Glow Wire Test | 750 °C @Thickness 0.800 mm |
1380 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
| Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
IEC 60695-2-12 |
| DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**) Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.20 mm |
1380 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
| Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
GWIT |
| LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
| Mitsubishi Xantar® C CF 107 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
| Glow Wire Test | 750 °C @Diameter 0.800 mm |
1380 °F @Diameter 0.0315 in |
GWFI; IEC 60695-2-12 |
| Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
GWIT |
| LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
GWFI/GWT |
| LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
GWIT |
| LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
GWFI/GWT |
| LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
| Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
| Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
| Glow Wire Test | 750 °C @Thickness 1.00 mm |
1380 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
| Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
| SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.50 mm |
1380 °F @Thickness 0.0591 in |
b.o. EDF HN60 E.02 |
| Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
b.o. EDF HN60 E.02 |
| Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
b.o. EDF HN60 E.02 |
| Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.20 mm |
1380 °F @Thickness 0.126 in |
VDE 0471/P2-4, IEC 695 |
| EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
VDE 0471/P2-4, IEC 695 |
| EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
VDE 0471/P2-4, IEC 695 |
| EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
| Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
Glow Wire Flammability Index GWFI; IEC 60695-2-12 |
| DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
| Glow Wire Test | 750 °C @Thickness 0.750 mm |
1380 °F @Thickness 0.0295 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.60 mm |
1380 °F @Thickness 0.0630 in |
Flammability Index; ICE 60695-12 |
| Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
| Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
| Glow Wire Test | 750 °C @Thickness 3.00 mm |
1380 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-12 |
| Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
| Glow Wire Test | 750 °C @Thickness 1.50 mm |
1380 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
| Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.50 mm |
1380 °F @Thickness 0.0591 in |
Ignition Temp; IEC 60695-2-12 |
| Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
| Glow Wire Test | 750 °C @Thickness 1.50 mm |
1380 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
| DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions... |
|||