| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
|
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
|
LG Chemical LUCON CP6080LP PC+CNT+GF
Description: Injection Molding, PC+CNT+GF, Electrostatic Dissipation, Low Surface TribochargeApplication: ATM parts, HDD BracketCAS No. 103598-77-2, 65997-17-3 and 7782-42-5Information provided by L..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
|
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
|
|||
| Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
|
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
|
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 290 °C | 554 °F | Injection molding; ISO 294 |
|
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber
PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
|
|||
| Melt Temperature | 290 °C | 554 °F | for test specimens; ISO 294 |
|
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced
High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
|
Covestro Makrolon® 1837* Polycarbonate, Impact Grade
ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable..
|
|||
| Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
|
Covestro Makrolon® 2656 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv..
|
|||
| Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
|
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp..
|
|||
| Melt Temperature | 290 °C | 554 °F | Injection Molding; ISO 294 |
|
Covestro Makrolon® T7855 Polycarbonate, Impact Grade
ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
|
|||
| Melt Temperature | 290 - 310 °C | 554 - 590 °F | |
|
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
|
|||