| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
|
PolyOne LubriOne™ NN-25GB/15T Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Plastcom SLOVAMID 6 GF 45 Polyamide 6, 45% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized
PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools..
|
|||
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
|
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre
FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
|
|||
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
Premix Thermoplastics PRE-ELEC® PBT 1455
PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel..
|
|||
| Mold Temperature | 40.0 - 90.0 °C | 104 - 194 °F | |
|
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Mold Temperature | 65.0 - 90.0 °C | 149 - 194 °F | |
|
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy
Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Start Point: 80°C |
|
Kingfa MAC-451PG Electroplating PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor..
|
|||
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber
SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded
Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
E-Polymers TEKAMID® HG10L 10% Glass Fiber Reinforced High Impact PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
|
|||
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection molding/Extrusion |
|
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
|
|||
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Injection Molding |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
|
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
|
|||
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
|
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry)
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF
|
|||
| Mold Temperature | 40.0 - 90.0 °C | 104 - 194 °F | |
|
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Information provided by Eurotec®
|
|||
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
|
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy
Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd.
|
|||