Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 800 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East)
Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T..
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Crastin® SK605 BK851 PBT  (Unverified Data**)
Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Glow Wire Test 800 °C

@Thickness 1.00 mm
1470 °F

@Thickness 0.0394 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 18 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 27 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 800 °C

@Diameter 1.50 mm
1470 °F

@Diameter 0.0591 in
GWFI; IEC 60695-2-12
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers
PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized
Glow Wire Test 800 °C

@Thickness 2.00 mm
1470 °F

@Thickness 0.0787 in
GWIT
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri..
Glow Wire Test 800 °C

@Thickness 2.00 mm
1470 °F

@Thickness 0.0787 in
GWIT
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi..
Glow Wire Test 800 °C

@Thickness 2.00 mm
1470 °F

@Thickness 0.0787 in
ignition temperature; EN 60695-2-13
Borealis Borcom™ WG140AI Polypropylene
Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good..
Glow Wire Test 800 °C

@Thickness 38.1 mm
1470 °F

@Thickness 1.50 in
GWFI; IEC 60695-12
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
GWFI; IEC 60695-2-12
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Glow Wire Test 800 °C

@Thickness 0.750 mm
1470 °F

@Thickness 0.0295 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Glow-Wire Ignition; IEC 60695-2-13
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
Glow Wire Test 800 °C

@Thickness 0.710 mm
1470 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
Glow Wire Test 800 °C

@Thickness 0.710 mm
1470 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
Glow Wire Test 800 °C

@Thickness 0.710 mm
1470 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Glow Wire Test 800 °C

@Thickness 0.710 mm
1470 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Glow Wire Test 800 °C

@Thickness 0.710 mm
1470 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
Glow Wire Test 800 °C

@Thickness 0.750 mm
1470 °F

@Thickness 0.0295 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Glow Wire Test 800 °C

@Thickness 3.00 mm
1470 °F

@Thickness 0.118 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Glow Wire Flammability Index; IEC 60695-2-12
Mitsubishi Xantar® 27 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Glow Wire Test 800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Copyright © lookpolymers.com All Rights Reserved