Polymer Property : Melting Point = 262 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
STN EN 11357-1
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber
PA66 for injection molding, reinforced with 20% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
Melting Point 262 °C
504 °F
10°C/min; DAM; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Melting Point 262 °C
504 °F
10°C/min; DAM; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Melting Point 262 °C
504 °F
10°C/min; DAM; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Melting Point 262 - 360 °C
504 - 680 °F
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Melting Point 262 °C
504 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Melting Point 262 °C
504 °F
ISO 11357
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi..
Melting Point 262 °C
504 °F
ISO 11357
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY
Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ..
Melting Point 262 °C
503 °F
Techmer ES HiFill® PA6/6 GF35 HS L 35% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and heat StabilizedProcessin..
Melting Point 262 °C
504 °F
ISO 11357
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
Melting Point 262 °C
504 °F
ASTM D3418
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p..
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Melting Point 262 °C
504 °F
DAM; ASTM D3418
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66
Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop..
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 KG30 NL 0B PA6.6, 30% glass fiber/glass bead reinforced, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info..
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 262 °C
504 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NA40 NL IX PA6.6, impact modified, natural
Information provided by Eurotec®
Melting Point 262 °C
504 °F
ISO 11357-1/3
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Melting Point 262 °C
504 °F
ISO 11357-1/3
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont..
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Melting Point 262 °C
504 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..