| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Plastcom PLASTAMID® 66 BT N 32 C PA66
PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber
PA66 reinforced with 20 % glass fiber, used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear w..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
PolyOne LubriOne™ NN-25GB/15T Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre
FeaturesChemically reinforced with 40% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. ..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre
FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 15 Polyamide 66, 15% Glass Fiber
FeaturesChemically reinforced with 15% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength
FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength ..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre
FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Melt Temperature | 265 - 300 °C | 509 - 572 °F | |
|
SABIC 6318B Linear Low Density Polyethylene for Cast Film
Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | Do not melt above 300°C |
|
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | DAM |
|
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | DAM |
|
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
|
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov..
|
|||
| Melt Temperature | 285 - 300 °C | 545 - 572 °F | Injection Molding |
|
LG Chemical LUPOY SC1004AU PC, High Impact
Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced
Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne..
|
|||
| Melt Temperature | 275 - 300 °C | 527 - 572 °F | |
|
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced
Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan..
|
|||
| Melt Temperature | 285 - 300 °C | 545 - 572 °F | ISO 294 |
|
Gromax BTE65-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET
Information provided by A. Schulman.
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
|
|||
| Melt Temperature | 270 - 300 °C | 518 - 572 °F | |
|
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
E-Polymers SEPAZ® LA40 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | Injection-molding/Extrusion |
|
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
|
|||
| Melt Temperature | 20.0 - 300 °C | 68.0 - 572 °F | Average value: 270 °C Grade Count:13 |
|
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
|
|||
| Melt Temperature | 260 - 300 °C | 500 - 572 °F | Injection Molding |
|
Styrolution Luran® S KR 2863 C UV Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
|
|||
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
|
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||