Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Extruded
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils. Typical Applications/End Uses: Typical uses include packaging films, monofilaments, bristles, rods, tubing and sheet.Availability:Asia PacificEuropeNorth America Features:General PurposeGasoline Resistance Good Chemical Resistance Good Melt StrengthGood ToughnessHigh RigidityHigh StrengthMedium ViscosityOil ResistantSolvent ResistantUses:Cast FilmFilmFood PackagingIndustrial ApplicationsMonofilamentsRodsSheetTubing Appearance: Natural ColorForms: PelletsProcessing Method: Injection Molding and ExtrusionInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 8.5 %

@Time 86400 sec
8.5 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; ISO 62
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
5.56 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 10.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
5.56 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C
500 °F
ISO 11357-3
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746
130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 85.0 °C

@Thickness 1.50 mm
185 °F

@Thickness 0.0591 in
UL 746
85.0 °C

@Thickness 3.00 mm
185 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Glow Wire Test 700 °C

@Thickness 1.50 mm
1290 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
700 °C

@Thickness 3.00 mm
1290 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
800 °C

@Thickness 1.50 mm
1470 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Thickness 0.750 mm
1.00e+14 ohm-cm

@Thickness 0.0295 in
IEC 60093
Dielectric Strength 23.0 kV/mm

@Thickness 1.00 mm
584 kV/in

@Thickness 0.0394 in
IEC 60243
Arc Resistance 60 - 119 sec

@Thickness 3.00 mm
60 - 119 sec

@Thickness 0.118 in
ASTM D495
Comparative Tracking Index 600 V

@Thickness 3.00 mm
600 V

@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
15 - 29 sec

@Thickness 3.00 mm
15 - 29 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI >= 120 arcs

@Thickness 1.50 mm
>= 120 arcs

@Thickness 0.0591 in
UL 746
>= 120 arcs

@Thickness 3.00 mm
>= 120 arcs

@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Processing Properties Metric English Comments
Zone 1 250 - 295 °C
482 - 563 °F
Zone 2 250 - 295 °C
482 - 563 °F
Zone 3 250 - 295 °C
482 - 563 °F
Zone 4 250 - 295 °C
482 - 563 °F
Zone 5 250 - 295 °C
482 - 563 °F
Die Temperature 270 - 295 °C
518 - 563 °F
Melt Temperature 270 - 295 °C
518 - 563 °F
Roll Temperature 20.0 - 80.0 °C
68.0 - 176 °F
Chill Roll Remperature
Descriptive Properties Value Comments
Blow Film Bath Temperature 20-80°C
Melt Pressure 3-17 MPa