Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.50 mm |
584 kV/in @Thickness 0.0984 in |
IEC 60243-1 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LATAN 13 S/30 30% Glass Sphere Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.00 mm |
584 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP1000S PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | Dielectric Breakdown Voltage, voltage rising rate = 1 kV/sec; JIS K-6911 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Europe-Africa-Middle East) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.59 mm |
584 kV/in @Thickness 0.0626 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo T-400 Nylon, 15% Glass-Reinforced Key Feature: G.F. 15%Information provided by Toyobo Co., Ltd |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | IEC 60243-1 |
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.59 mm, Temperature 25.0 °C |
584 kV/in @Thickness 0.0625 in, Temperature 77.0 °F |
|
Cytec EN-14 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | ASTM D149 |
Asahi Glass AFLAS® 100H TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 23.0 kV/mm | 584 kV/in | |
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |