Polymer Property : CTE, linear, Transverse to Flow = 10.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 10.0 - 110 µm/m-°C
5.56 - 61.1 µin/in-°F
Average value: 66.2 µm/m-°C Grade Count:21
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Temperature 55.0 - 160 °C
5.56 µin/in-°F
<br>@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
5.56 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6 &nbsp;(Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
CTE, linear, Transverse to Flow 10.0 - 80.0 µm/m-°C
5.56 - 44.4 µin/in-°F
Average value: 33.3 µm/m-°C Grade Count:3
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
CTE, linear, Transverse to Flow 10.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..