Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 200 - 230 °C | 392 - 446 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® C 206 PA6, DRY Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, DRY Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0 Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® C 402 M PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high .. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® C 52G1 V20 PA6, DRY Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® C 52G3 MZ25 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosph.. |
|||
Feed Temperature | 210 - 230 °C | 410 - 446 °F | |
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C216V15 15% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C216V25 25% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C216V30 30% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY Description: Polyamide PA6 reinforced with 33% of glass fiber, heat stabilized, containing recycled material.Available in: North AmericaProduct Applications: This grade is suitable for none critical.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black... |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® PSB 286 PA6, DRY Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Feed Temperature | 225 - 230 °C | 437 - 446 °F | |
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a.. |
|||
Feed Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America.. |