Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer Lavergne Performance Compounds
Trade Name VYTEEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temperature -Daimler Chrysler MSMB-206 type II compliantTypical Applications: -Automotive -Structural frames -AppliancesInformation provided by Bieglo Gmbh for Lavergne Performance Compounds
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Ash 16 %
16 %
ASTM D2854
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
5 mm/min; ASTM D638
Flexural Strength 140 MPa
20300 psi
1.3 mm/min; ASTM D790
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.850 J/cm

@Temperature -29.0 °C
1.59 ft-lb/in

@Temperature -20.2 °F
ASTM D256
0.930 J/cm

@Temperature 23.0 °C
1.74 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ASTM D648
Flame Spread 100 mm/min
3.94 in/min
SAE J 369
Processing Properties Metric English Comments
Feed Temperature 200 - 230 °C
392 - 446 °F
Middle Barrel Temperature 240 - 250 °C
464 - 482 °F
Front Barrel Temperature 260 - 275 °C
500 - 527 °F
Nozzle Temperature 270 - 280 °C
518 - 536 °F
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Users viewing this material also viewed the following: