Solvay TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA6 reinforced with 33% of glass fiber, heat stabilized, containing recycled material.Available in: North AmericaProduct Applications: This grade is suitable for none critical and less demanding parts. This product is available in black. This product can only be used in line with the specific recommendations of the Rhodia Engineering Plastics customer technical service. Rhodia Engineering Plastics declines all responsibilities for all problems caused by the use of this product, not in line with the recommendations of Rhodia Engineering Plastics customer technical serviceInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength at Break 189.3 MPa
27460 psi
ISO 527 Type 1A
Elongation at Break 3.3 %
3.3 %
ISO 527 Type 1A
Tensile Modulus 10.7 GPa
1550 ksi
ISO 527 Type 1A
Flexural Strength 285 MPa
41300 psi
ISO 178
Flexural Modulus 9.088 GPa
1318 ksi
ISO 178
Izod Impact, Notched (ISO) 15.5 kJ/m²
7.38 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/1U
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Processing Properties Metric English Comments
Feed Temperature 225 - 230 °C
437 - 446 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 230-240°C
Mixing Zone 240-250°C