Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for the manufacturing of complicated small as well as large surface mouldings. Possible for wall thickness from 0.5mm. High grade surface brightness also at colored types. Delivered in natural and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0145 cm/cm
0.0145 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0152 cm/cm
0.0152 in/in
STN 64 0808
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
STN EN ISO 527-2
Elongation at Break 4.0 %
4.0 %
STN EN ISO 527-2
Tensile Modulus 2.75 GPa
399 ksi
STN EN ISO 527-2
Flexural Strength 95.0 MPa
13800 psi
STN EN ISO 178
Flexural Modulus 3.00 GPa
435 ksi
STN EN ISO 178
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -20.0 °C
23.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
STN EN ISO 75/A
Vicat Softening Point 200 °C
392 °F
B; STN EN ISO 306
Flammability, UL94 V-0
V-0
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
STN IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
STN IEC 60243
Comparative Tracking Index 500 V
500 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 100 MPa
10200 - 14500 psi
Users viewing this material also viewed the following: