Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 51 T 30 PP, 30% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S CP400 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 LI LS PA6, improved strength, light stability FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application .. |