Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Celanese FORTRON 1342L4 PPS, 40% Specialty
(Unverified Data**) Fortron 1342L4 is a low wear grade, ideally suited for bearings, gears and other sliding friction/wear applications. This product is glass fiber reinforced and contains PTFE.40% Glass reinforced wit.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® A TA4AOZ Thermoplastic Elastomer, Outdoor application with adhesion to PC, PC/ABS and optimized scratch resistance The UV/AD1 Series is recommended for applications requiring a high UV resistance and adhesion to polar thermoplastics such as PC, ABS, PC/ABS. It is particularly appropriate for automotive exterior .. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC4PCN Thermoplastic Elastomer, Adhesion to PA, optimized compression set The AD/PA/CS Series is recommended for applications with excellent adhesion to PA as well as outstanding compression set. The compounds are available in natural and black colors. Typical application.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC4PCZ Thermoplastic Elastomer, Adhesion to PA, optimized compression set The AD/PA/CS Series is recommended for applications with excellent adhesion to PA as well as outstanding compression set. The compounds are available in natural and black colors. Typical application.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC5NYN Thermoplastic Elastomer, Adhesion to PA The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | Injection |
Kraiburg TPE THERMOLAST® K TC6CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC7NYN Thermoplastic Elastomer, Adhesion to PA The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC7NYZ Thermoplastic Elastomer, Adhesion to PA The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC7SCE Thermoplastic Elastomer, high scratch resistance The SCR Series is recommended for applications requiring a high degree of scratch resistance. The series is characterized, among other things, by a pleasant feel. Typical applications: Car matsFunct.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | Injection |
Kraiburg TPE THERMOLAST® K TP6LDZ Thermoplastic Elastomer, Low Density, Automotive Exterior Applications The UV/LD/b Series is recommended for applications requiring high UV resistance. It is particularly appropriate for automotive exterior. Typical applications: Cowls gasketsRoof rimsWater deflectorsW.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC0LEZ Thermoplastic Elastomer, UV resistance The UV/FG Series is recommended for applications requiring high UV resistance. It is particularly appropriate for automotive exterior and interior components. Typical applications: Cowls gasketsRoof.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC7HBZ Thermoplastic Elastomer The AD/POM Series is recommended for applications with excellent adhesion to POM. The compounds are available in natural and black colors. Typical applications: BumpersFunction and design elementsGr.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | Injection |
Kraiburg TPE THERMOLAST® K TC8CSZ Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TC8HAA Thermoplastic Elastomer The AD/POM Series is recommended for applications with excellent adhesion to POM. The compounds are available in natural and black colors. Typical applications: BumpersFunction and design elementsGr.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TF2CGN Thermoplastic Elastomer, Natural The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TF2CGT Thermoplastic Elastomer, Translucent The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TF3FMS Thermoplastic Elastomer, adhesion to PC, ABS, PETG The FC/AD1 Series is recommended for applications with food contact providing excellent adhesion to polar thermoplastics such as PC, ABS and PETG. Typical applications:Function and design elementsGr.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® M TM6ADT Thermoplastic Elastomer, for medical and pharmaceutical technology The MC/AD1 Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The series is characterized by excellent adhesion pro.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Celanese FORTRON 6150T6 PPS, 50% Specialty Fortron 6150T6 is a 50% glass-fiber reinforced and mineral-filled grade with improved impact and heat shock resistance.Information provided by Celanese |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | Injection |
Kraiburg TPE THERMOLAST® K TC8FRN Thermoplastic Elastomer, Flame retardant The FR Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Seals for.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TF0STT Thermoplastic Elastomer, very low rubber hardness The FC/ht Series is a highly transparent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP. Typical applications:.. |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Kraiburg TPE THERMOLAST® K TF1STL Thermoplastic Elastomer, very low rubber hardness The FC/ht Series is a highly transparent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP. Typical applications:.. |
|||
Injection Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
Celanese FORTRON 6450A6 PPS, 51% Specialty Fortron 6450A6 is a fiberglass reinforced, mineral filled alloy that exhibits improved wear and sliding properties versus standard Fortron compounds.Information provided by Celanese |
|||
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | Injection |
Kraiburg TPE THERMOLAST® K TP5VCZ Thermoplastic Elastomer, Adhesion to PC, ABS, PETG, optimized compression set The AD1/CS Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS as well as excellent compression set. The compounds are available in natu.. |