Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 GF 15 T 15 TS PA66 reinforced with glass fibers and mineral filler, heat stabilized Black PA66 for injection molding, reinforced with 15% glass fiber and 15% mineral filler, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of elect.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 15 T 25 TS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber Information provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radiflam® S RV300AE (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV300 990 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(d The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Improved thermal stabilization. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
|
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® TV4 261 SF PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant, High Flow |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® TV6 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 NL FA 50 PA 6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good.. |