Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.20 - 1.58 g/cc
0.0434 - 0.0571 lb/in³
Average value: 1.37 g/cc Grade Count:21
Filler Content 5.00 - 40.0 %
5.00 - 40.0 %
Average value: 16.4 % Grade Count:16
Water Absorption 0.120 - 0.200 %
0.120 - 0.200 %
Average value: 0.133 % Grade Count:12
Additive Loading 15.0 - 40.0 %
15.0 - 40.0 %
Average value: 26.3 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:21
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.9 - 179 MPa
10000 - 26000 psi
Average value: 107 MPa Grade Count:21
Elongation at Break 0.500 - 5.00 %
0.500 - 5.00 %
Average value: 1.79 % Grade Count:21
Modulus of Elasticity 5.86 - 22.1 GPa
850 - 3200 ksi
Average value: 10.4 GPa Grade Count:21
Flexural Yield Strength 103 - 248 MPa
15000 - 36000 psi
Average value: 154 MPa Grade Count:21
Flexural Modulus 4.83 - 19.3 GPa
700 - 2800 ksi
Average value: 9.22 GPa Grade Count:21
Izod Impact, Notched 0.534 - 2.67 J/cm
1.00 - 5.00 ft-lb/in
Average value: 0.778 J/cm Grade Count:21
Izod Impact, Unnotched 1.87 - 6.14 J/cm
3.50 - 11.5 ft-lb/in
Average value: 3.36 J/cm Grade Count:19
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 - 149 °C
275 - 300 °F
Average value: 144 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 129 - 149 °C
265 - 300 °F
Average value: 139 °C Grade Count:10
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:13
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 100 ohm-cm
1.00 - 100 ohm-cm
Average value: 23.3 ohm-cm Grade Count:20
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 79600 ohm Grade Count:20
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.84 sec Grade Count:19
Processing Properties Metric English Comments
Processing Temperature 249 - 293 °C
480 - 560 °F
Average value: 277 °C Grade Count:12
Melt Temperature 288 - 338 °C
550 - 640 °F
Average value: 304 °C Grade Count:9
Mold Temperature 65.6 - 121 °C
150 - 250 °F
Average value: 97.0 °C Grade Count:21
Drying Temperature 121 - 121 °C
250 - 250 °F
Average value: 121 °C Grade Count:9
Moisture Content 0.0200 %
0.0200 %
Average value: 0.0200 % Grade Count:8
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:8
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:20