Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Network Polymers Nylon 6G20L
Description: Natural NylonInformation provided by Network Polymers Inc.
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated  (discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 4.83 GPa

@Temperature 22.8 °C
700 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 3200-2FC PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated  (discont
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 4.83 - 8.96 GPa
700 - 1300 ksi
Average value: 6.48 GPa Grade Count:15
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 3204  Ethylene Tetrafluoroethylene (ETFE) Glass Fiber 25%  (discontinued **)
Glass Fiber 25%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 204F  Nylon 12 (PA 12) Glass Fiber 25%  (discontinued **)
Glass Fiber 25%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Modulus 4.83 GPa
700 ksi
Tangent; ASTM D790
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 4.83 GPa
700 ksi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled
13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc.
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Global XNY-577 20% Reinforced Polycarbonate/Polyester Alloy
Information provided by Global Polymers Corporation.
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill® ASA GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF/B30 A1 10/20% Glass Bead/Glass Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lu..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company EMI 2163 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 202 A HS Nylon 6 (PA), Glass Fiber - Heat Stabilized
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 2200 LF AR 15 TFE 15 Polyetheretherketone (PEEK), Aramid Fiber - PTFE Lubricated
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 1300 AR 15 TFE 15 SI 2 Polyphenylene Sulfide (PPS), Aramid Fiber Reinforced - PTFE & Silicone Lubricated
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 203 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 2101 LF Polyetherimide (PEI), Glass Fiber - Low Flow
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Ensinger Tecapeek® XP-102 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled
Data provided by Clariant Masterbatches
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced
Information provided by Asahi Thermofil
Flexural Modulus 4.83 GPa

@Temperature 71.1 °C
700 ksi

@Temperature 160 °F
ASTM D790
Celanese Celcon® GC25A POM, 25% Glass Reinforced
Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 201D GB 20  Nylon 6/12 (PA 6/12) Glass Fiber 10% - Glass Bead 20%  (disconti
Glass Fiber 10% - Glass Bead 20%Comments:Glass FiberGlass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 201B  Nylon 6/10 (PA 6/10) Glass Fiber 10%  (discontinued **)
Glass Fiber 10%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 1402 N Z  Polyethersulfone (PES) Glass Fiber 15% - FDA Type - High Viscosity &nbs
Glass Fiber 15% - FDA Type - High ViscosityComments:Glass FiberFDA CompliantHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 499 X 87338 Polystyrene (PS), Glass Fiber - Permanently Anti-static
Copyright © lookpolymers.com All Rights Reserved