Polymer Property : Mold Temperature = 250 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 82.2 - 121 °C
180 - 250 °F
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Mold Temperature 76.7 - 121 °C
170 - 250 °F
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 301 TFE 15 FR L Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP 301 TFE FR L series of compounds incorporate various percentages of PTFE into a glass fiber reinforced polycarbonate base which also includes external lubricants for enhanced processing. Th..
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 303 TFE 10 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 303 TFE 15 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 381 Polycarbonate (PC), Carbon Fiber
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 381 TFE 13 SI 2 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 381 TFE 15 Polycarbonate (PC) Carbon Fiber - PTFE Lubricated - UL94 HB
Mold Temperature 91.0 - 121 °C
196 - 250 °F
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber  (discontinued **)
Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur..
Mold Temperature 65.6 - 121 °C
150 - 250 °F
RTP Company VLF 81005 Polybutylene Terephthalate (PBT), Long Glass Fiber
Mold Temperature 93.3 - 121 °C
200 - 250 °F
generally preferred range, may vary with thickness
Celanese Celcon® M15HP POM  (Unverified Data**)
Celcon® acetal copolymer grade M15HP is a creep resistant, high viscosity polymerStandard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high com..
Mold Temperature 93.3 - 121 °C
200 - 250 °F
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement  (discontinued *
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Mold Temperature 93.3 - 121 °C
200 - 250 °F
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Mold Temperature 65.6 - 121 °C
150 - 250 °F
RTP Company RTP 3499-3 X 90363  Liquid Crystal Polymer (LCP) Thermally Conductive - Electrically Conductive
Thermally Conductive - Electrically ConductiveComments:Thermally ConductiveElectrically ConductiveUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can ..
Mold Temperature 71.1 - 121 °C
160 - 250 °F
RTP Company EMI 330 F FR Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Mold Temperature 71.1 - 121 °C
160 - 250 °F
RTP Company EMI 331 E FR Polycarbonate (PC) 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company ESD 385 Polycarbonate (PC); Carbon Fiber - Electrically Conductive
Mold Temperature 71.1 - 121 °C
160 - 250 °F
RTP Company RTP 2000 A-670 Polysulfone ABS Alloy
Mold Temperature 93.3 - 121 °C
200 - 250 °F
RTP Company RTP 2382 C Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 300 HB Polycarbonate (PC), Unreinforced - UL94 HB
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 300 MG 30 Polycarbonate (PC), Milled Glass
Mold Temperature 79.4 - 121 °C
175 - 250 °F
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized
Data provided by Clariant Masterbatches
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 1105 TFE 15 Polyethylene Terephthalate (PET), Glass Fiber Reinforced - PTFE Lubricated
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 307 TFE 15 Polycarbonate (PC), Glass Fiber - PTFE Lubricated
Mold Temperature 65.6 - 121 °C
150 - 250 °F
RTP Company RTP 3405-3 Liquid Crystal Polymer (LCP), Glass Fiber
Liquid crystal polymers offer outstanding heat and chemical resistance and are inherently ignition resistant. The unique self-reinforcing crystalline structure allows a molding cycle that is faster..
Mold Temperature 65.6 - 121 °C
150 - 250 °F
RTP Company RTP 3405-3 TFE 15 Liquid Crystal Polymer (LCP), Glass Fiber - PTFE Lubricated
Mold Temperature 65.6 - 121 °C
150 - 250 °F
RTP Company RTP 3499-3 X 113393 C Liquid Crystal Polymer (LCP) Glass Fiber - LDS Platable
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 387 Polycarbonate (PC), Carbon Fiber
Mold Temperature 82.2 - 121 °C
180 - 250 °F
RTP Company RTP 399 X 115084 A Polycarbonate (PC), Carbon Nanotube - Electrically Conductive - ESD Protection - High Purity
Mold Temperature 110 - 121 °C
230 - 250 °F
Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced  (Unverified Data**)
Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c..