Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 - 149 °C | 185 - 300 °F | Average value: 112 °C Grade Count:18 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 135 - 149 °C | 275 - 300 °F | Average value: 144 °C Grade Count:8 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 132 - 149 °C | 270 - 300 °F | ASTM D648 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 136 - 149 °C | 277 - 300 °F | Average value: 145 °C Grade Count:46 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 - 149 °C | 165 - 300 °F | Average value: 99.8 °C Grade Count:12 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 - 149 °C | 250 - 300 °F | Average value: 141 °C Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.2 - 149 °C | 207 - 300 °F | Average value: 122 °C Grade Count:21 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 101 - 149 °C | 214 - 300 °F | Average value: 129 °C Grade Count:24 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |