Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 1.87 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.87 - 8.81 J/cm
3.50 - 16.5 ft-lb/in
Average value: 5.96 J/cm Grade Count:6
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 1.87 - 6.14 J/cm
3.50 - 11.5 ft-lb/in
Average value: 3.36 J/cm Grade Count:19
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched 1.87 J/cm

@Thickness 3.17 mm
3.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrafil® J-1200/CF/10 ABS, 10% Carbon Fiber Reinforced
Izod Impact, Unnotched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive)
Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32..
Izod Impact, Unnotched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 1.87 - 7.47 J/cm
3.50 - 14.0 ft-lb/in
Average value: 5.99 J/cm Grade Count:16
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Unnotched 1.87 - 10.7 J/cm
3.50 - 20.0 ft-lb/in
Average value: 4.43 J/cm Grade Count:13
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved