Mechanical Properties Metric English Comments
Izod Impact, Notched <= 0.534 J/cm

@Temperature 22.8 °C
<= 1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1102  Polyethylene Terephthalate (PET) Glass Fiber 15%  (discontinued **)<
Glass Fiber 15%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 800 TFE 20 DEL Acetal (POM), Homopolymer - PTFE Lubricated - UL94 HB
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Izod Impact, Notched 0.534 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® AT-10GB/000 Black Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.534 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® AS-10CF/000 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued
Description/Features:Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.18 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
Izod Impact, Notched 0.534 - 0.747 J/cm
1.00 - 1.40 ft-lb/in
Average value: 0.651 J/cm Grade Count:5
Overview of materials for Nylon 11 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6/6 FR 144
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Halogen Free, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ABS HI 0300 High Impact
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by ..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GF7 L 7% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 7% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6 E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6
Information provided by A. Schulman.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company PermaStat® 1800 Acrylic (PMMA), Permanently Anti-static - ESD Protection
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 105 HB Polypropylene (PP), Glass Fiber - UL94 HB
RTP 105 HB offers an excellent balance of rigidity, strength and dimensional stability combined with good heat and chemical resistance.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1084 TFE 15 Polybutylene Terephthalate (PBT), Carbon Fiber - PTFE Lubricated
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 299 A X 108950 G Nylon 6 (PA), High Gravity Compound
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 6 GF15H 15% Glass Bead Reinforced, Heat Stabilized Nylon 6
Information provided by A. Schulman.
Izod Impact, Notched 0.534 J/cm

@Thickness 3.20 mm
1.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company EMI 862 Acetal (POM) Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1387 P-1 Polyphenylene Sulfide (PPS), Carbon Fiber
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Celanese CELANEX 2001 PBT, Unfilled
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Izod Impact, Notched 0.534 - 0.854 J/cm
1.00 - 1.60 ft-lb/in
Average value: 0.667 J/cm Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Izod Impact, Notched 0.534 - 1.87 J/cm
1.00 - 3.50 ft-lb/in
Average value: 1.27 J/cm Grade Count:38
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6 GF15 FR-N 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, Halog..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 2103 Z  Polyetherimide (PEI) Glass Fiber 20% - FDA Type  (discontinued **)&l
Glass Fiber 20% - FDA TypeComments:Glass Fiber FDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4000 TFE 18 SI 2  Polyphthalamide (PPA) PTFE 18% - Silicone 2%  (discontinue
PTFE 18% - Silicone 2%Comments:PTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pro..
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PBT GF15 FR X 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, In..