Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 288 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 288 - 316 °C
550 - 601 °F
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PPX-GP1 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Melt Temperature 288 - 316 °C
550 - 600 °F
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 288 - 321 °C
550 - 610 °F
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 301 TFE 10 Polycarbonate (PC), Glass Fiber - PTFE Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 303 L Polycarbonate (PC), Glass Fiber - Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 303 TFE 10 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 307 SI 2 Polycarbonate (PC), Glass Fiber - Silicone Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 381 Polycarbonate (PC), Carbon Fiber
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 383 HEC Polycarbonate (PC), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 385 TFE 10 SI 2 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 127605 Polycarbonate (PC) Glass Fiber - Flame Retardant
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Melt Temperature 288 - 343 °C
550 - 650 °F
Average value: 318 °C Grade Count:14
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Melt Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
Melt Temperature 288 - 316 °C
550 - 601 °F
Styron EMERGEâ„¢ 4530-10 Polycarbonate
EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Melt Temperature 288 - 316 °C
550 - 601 °F
Styron EMERGEâ„¢ 4702-15 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res..
Melt Temperature 288 - 310 °C
550 - 590 °F
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company ESD 300 EM TFE 15 Polycarbonate (PC), ESD Protection - Static Dissipative - Easy Molding - PTFE Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company ESD 301 EM Polycarbonate (PC), Glass Fiber - ESD Protection - Static Dissipative - Easy Molding
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 FR A UV Polycarbonate (PC), Unreinforced - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP 300 FR A family of materials offer dimensional stability, rigidity, heat resistance and excellent impact strength. RTP 300 FR A UV is a UV stabilized grade.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 GB 20 Polycarbonate (PC), Glass Bead
Melt Temperature 288 - 315 °C
550 - 599 °F
Extrusion Coating Processability
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult..
Melt Temperature 288 °C
550 °F
Chem Polymer Chemlon 140 M Nylon 66, 40% Mineral Reinforced
A 40% mineral reinforced nylon 66 exhibiting excellent stiffness in parts where control of warpage is essential.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 302 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 305 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 305 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance an..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 301 EM L HB Polycarbonate (PC), Glass Fiber - Easy Molding - Lubricated - UL94 HB
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 102186 Polycarbonate (PC), Carbon Fiber - Glass Fiber
Copyright © lookpolymers.com All Rights Reserved