Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000400 - 0.00300 cm/cm
0.000400 - 0.00300 in/in
Average value: 0.00157 cm/cm Grade Count:13
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00183 cm/cm Grade Count:9
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage 0.00200 - 0.00300 cm/cm
0.00200 - 0.00300 in/in
Average value: 0.00269 cm/cm Grade Count:8
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage 0.00200 - 0.00300 cm/cm
0.00200 - 0.00300 in/in
Average value: 0.00267 cm/cm Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00146 cm/cm Grade Count:15
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Linear Mold Shrinkage 0.000100 - 0.00300 cm/cm
0.000100 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:21
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00100 - 0.00300 cm/cm
0.00100 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:5
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.000 - 0.00300 cm/cm
0.000 - 0.00300 in/in
Average value: 0.00100 cm/cm Grade Count:19
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Linear Mold Shrinkage 0.00250 - 0.00300 cm/cm
0.00250 - 0.00300 in/in
Average value: 0.00275 cm/cm Grade Count:10
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.00150 - 0.00300 cm/cm
0.00150 - 0.00300 in/in
Average value: 0.00213 cm/cm Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Linear Mold Shrinkage 0.00300 - 0.00300 cm/cm

@Temperature 80.0 - 80.0 °C
0.00300 - 0.00300 in/in

@Temperature 176 - 176 °F
Average value: 0.00300 cm/cm Grade Count:2
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.000500 - 0.00300 cm/cm
0.000500 - 0.00300 in/in
Average value: 0.00150 cm/cm Grade Count:7
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage 0.00100 - 0.00300 cm/cm
0.00100 - 0.00300 in/in
Average value: 0.00221 cm/cm Grade Count:9
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..