Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 4.83 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.83 GPa
701 ksi
ASTM D790
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 1300.5  Polyphenylene Sulfide (PPS) Glass Fiber 5%  (discontinued **)
Glass Fiber 5%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for t..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 1300 AR 15 SI 2  Polyphenylene Sulfide (PPS) Aramid Fiber 15% - Silicone 2%  
Aramid Fiber 15% - Silicone 2%Comments:Aramid FiberSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio..
Flexural Modulus 4.83 GPa

@Temperature 22.8 °C
700 ksi

@Temperature 73.0 °F
ASTM D790
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 4000 AR 15 Polyphthalamide (PPA), Aramid Fiber
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
RTP Company RTP 1701 MG 20  Modified Polyphenylene Oxide (PPO) Glass Fiber 10% - Milled Glass 20% &am
Glass Fiber 10% - Milled Glass 20%Comments:Glass FiberMilled GlassUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pr..
Flexural Modulus 4.83 GPa
700 ksi
Tangent; ASTM D790
Fiberfil® J-60/30/E4 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 4.83 GPa
700 ksi
MTI ThermoStran® PP-30G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill® PA6 CM30 L 30% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composit..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 GF10 TL10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(5%)Features: Lubricated, Good Wear Resistance, Low Fricti..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES HiFill® PBT GF15 WT 096 LE 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: WhiteTPCI# 6862111Information provided by TP Composit..
Flexural Modulus 4.83 GPa
701 ksi
Method I (3 point load), 2.0 mm/min; ASTM D790
Styron CALIBREâ„¢ 5201-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5201-8 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALIB..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Techmer ES Luriblend® POM CO GM30 TL5 30% Glass Milled Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Compos..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Chase Plastics CP Pryme® N130GL (COND, 50% RH) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company EMI 331.25 D FR Polycarbonate (PC), 12.5% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 103 FR A Polypropylene (PP), Glass Fiber - Flame Retardant - Non-PBB/PBDE
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 202 Nylon 6/6 (PA), Glass Fiber
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 2101 Polyetherimide (PEI), Glass Fiber
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Celanese CELANEX 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced
Information provided by Asahi Thermofil
Flexural Modulus 4.83 GPa
701 ksi
ASTM Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.
Flexural Modulus 4.83 GPa

@Temperature 71.1 °C
700 ksi

@Temperature 160 °F
ASTM D790
Celanese Celcon® GC25A POM, 25% Glass Reinforced
Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower..
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 1002 TFE 15 Z Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated - FDA Compliant Ingredients
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 299 A X 92682 D Nylon 6 (PA), High Gravity Compound - Easy Molding
Flexural Modulus 4.83 GPa

@Temperature 22.8 °C
700 ksi

@Temperature 73.0 °F
ASTM D790
Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP 2299 X 115090 B Polyetheretherketone (PEEK), Carbon Nanotube - Electrically Conductive
Flexural Modulus 4.83 GPa
700 ksi
ASTM D 790
RTP Company RTP PA66 13 GF BLK Nylon 6/6 (PA), Value Product - Glass Fiber - Heat Stabilized
Copyright © lookpolymers.com All Rights Reserved