Processing Properties Metric English Comments
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced
Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified
Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow
Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F
Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 TFE 18 SI 2 Polycarbonate (PC), PTFE Lubricated - Silicone Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 302 Polycarbonate (PC) Glass Fiber
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 302 TFE 15 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 303 TFE 15 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 384 HEC Polycarbonate (PC), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection
Melt Temperature 288 - 304 °C
550 - 579 °F
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Melt Temperature 288 - 310 °C
550 - 590 °F
RTP Company RTP 4099 X 113516 A Polyphthalamide (PPA) Glass Fiber - Flame Retardant - Halogen Free
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Melt Temperature 288 - 304 °C
550 - 580 °F
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened
Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Melt Temperature 288 - 316 °C
550 - 600 °F
Average value: 302 °C Grade Count:5
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Melt Temperature 288 - 316 °C
550 - 601 °F
Stock
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Melt Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1510R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Melt Temperature 288 - 316 °C
550 - 601 °F
Styron EMERGEâ„¢ 4702-8 Polycarbonate
EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi..
Melt Temperature 288 - 316 °C
550 - 601 °F
Styron EMERGEâ„¢ 4731-8 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability ..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 AR 10 TFE 15 Polycarbonate (PC), Aramid Fiber - PTFE Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 SI 2 Polycarbonate (PC), Silicone Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 303 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance an..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 305 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance an..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 305 TFE 10 Polycarbonate (PC), Glass Fiber - PTFE Lubricated
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 381 FR Polycarbonate (PC), Carbon Fiber - Flame Retardant
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 120436 C Polycarbonate (PC), Carbon Nanotube
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 301 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. ..
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 304 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance an..