Polymer Property : Static Decay = 0.500 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Static Decay 0.500 sec
0.500 sec
Average value: 0.500 sec Grade Count:4
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.77 sec Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.84 sec Grade Count:19
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 0.875 sec Grade Count:4
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.81 sec Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:9
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.00 sec Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:3
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved