Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 121 °C | 250 °F | |
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 300 TFE 15 SI 2 Polycarbonate (PC), PTFE Lubricated - Silicone Lubricated |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company RTP 301 FR UV Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. .. |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 305 TFE 15 Polycarbonate (PC), Glass Fiber - PTFE Lubricated |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company RTP 382 HEC FR Polycarbonate (PC) Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection - Flame Retardant |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 800 Acetal (POM), Base Resin |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 800 MS 3 Acetal (POM), Molybdenum Disulfide |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 840 Acetal (POM), Mineral |
|||
Drying Temperature | 121 °C @Time 7200 sec |
250 °F @Time 2.00 hour |
|
RTP Company RTP 899 X 120422 D Acetal (POM), Carbon Nanotube - ESD Protection |
|||
Drying Temperature | 121 °C | 250 °F | Average value: 121 °C Grade Count:5 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Drying Temperature | 121 °C | 250 °F | |
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |
|||
Drying Temperature | 121 °C | 250 °F | |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 121 °C | 250 °F | |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company EMI 333 D FR Polycarbonate (PC) 20% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 1007 SI 2 Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - Silicone Lubricated |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company RTP 1099 X 117938 B Polybutylene Terephthalate (PBT) Wear Alloy - APWA (All Polymeric Wear Additive) |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 1378 CL Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company ESD 1085 Polybutylene Terephthalate (PBT), Carbon Fiber - Electrically Conductive |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company RTP 2099 X 128018 A Polycarbonate/Polyester; Glass Fiber - Carbon Fiber - Electrically Conductive |
|||
Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
LNP Thermocomp® JF-1006 BK8-115 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 3200 MG 20 Ethylene Tetrafluoroethylene (ETFE), Milled Glass |
|||
Drying Temperature | 121 °C @Time 14400 sec |
250 °F @Time 4.00 hour |
|
RTP Company RTP 385 TFE 15 SI 2 Polycarbonate (PC); Carbon Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 800 Z Acetal (POM), FDA Compliant Ingredients |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 804 TFE 15 Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated |
|||
Drying Temperature | 121 °C | 250 °F | |
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 121 °C | 250 °F | |
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone
(disconti Data provided by PolyOne. |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 1002 TFE 15 Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 300 TFE 20 Polycarbonate (PC), PTFE Lubricated |
|||
Drying Temperature | 121 °C | 250 °F | |
RTP Company RTP 304 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2 The RTP 300 SE series represent a range of glass fiber reinforced, self-extinguishing polycarbonate materials which offer outstanding dimensional stability with improved rigidity, heat resistance an.. |