| Category | Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass SMC |
| Manufacturer | Menzolit |
| Trade Name | Menzolit® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.80 g/cc | 0.0650 lb/in³ | ISO 1183 |
| Water Absorption | <= 0.50 % | <= 0.50 % | ISO 62 |
| Linear Mold Shrinkage | 0.00080 cm/cm | 0.00080 in/in | ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
| Tensile Strength, Yield | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
| Elongation at Yield | 0.00 % | 0.00 % | tensile rupture strain; ISO 527-4 |
| Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
| Flexural Strength | 150 MPa @Temperature 22.0 °C |
21800 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
| Flexural Modulus | 11.0 GPa @Temperature 22.0 °C |
1600 ksi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
| Poissons Ratio | 0.30 | 0.30 | |
| Shear Modulus | 4.60 GPa | 667 ksi | in plane |
| Charpy Impact, Notched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
| Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
| Thermal Conductivity | 0.700 W/m-K | 4.86 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 165 °C | 329 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | >= 200 °C | >= 392 °F | ISO 75-2 |
| Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
| Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
| Flammability, UL94 | V-0 @Thickness 3.00 mm |
V-0 @Thickness 0.118 in |
|
| Oxygen Index | 43 % | 43 % | ISO 4589-2 |
| Glow Wire Test | 960 °C | 1760 °F | IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Constant | 4.0 | 4.0 | IEC 60250 |
| Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.010 | 0.010 | IEC 60250 |
| Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |