Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 502AU (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 9704S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70H Ethylene Propylene Rubber Peroxide cured, white Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Fede.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E80B Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistan.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering N65E Nitrile Rubber Nitrile Butadiene Rubber (NBR) 62-72 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5509 Grade C (inactive for new de.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering N70F Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering N70L Nitrile Rubber Nitrile Butadiene Rubber (NBR), 70 °IRHD. Low- Med acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet: ASTM D2000/SAE J200 line call-out: M5BG710, A14, B14, EO14, EO34.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering N70U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade A1 (specification inactive for new design).Application.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering R70Z Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to meet BS1154 Grade Z70. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Chomerics |
Parker Chomerics CHO-MASK II HT Conductive Foil Tape The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Flex TR10 |
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering C60W Chloroprene Rubber Off-white, Chloroprene Rubber, 56-65 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Saint-Gobain T-Bond II® Semi-Rigid Polyurethane Foam Structural Glazing and Cladding Spacer System Description: Semi-Rigid Polyurethane Foam Substrate used as a Structural Glazing and Cladding Spacer System for In-Shop Fabrication. Semi-Rigid Polyurethane: An open cell structure allows air and mo.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg R320 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg T620 Butyl Rubber Butyl rubber is a copolymer of isobutylene and a small percentage of isoprene.PropertiesWith careful compounding Butyl has really good tensile strength.Butyl has very low permeability to air and oth.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Loctite® Shadowcure™ 394 Acrylic/urethane UV Coating Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Dow Corning XIAMETER® PMCPPMX-200 12,500CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 12,500CS. 100% active, 12,500 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Dow Corning XIAMETER® PMCPPMX-200 1000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 1,000CS. 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
ChevronTexaco Black Pearl® NLGI 0 Grease EP FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-HD EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg R847 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |