Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | IES 1006 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 2400 Unsaturated Polyester UP BMC 2400 is a general purpose BMC for applications in the field of low smoke density and non toxic smoke.. The flammability meets the demands of EN45545 and is classified according to British standa.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-3284 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-40 Electronic Liquid 3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-43 Electronic Liquid 3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-72 Electronic Liquid 3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |