Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 140C (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 368F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 374C (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 760H (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70H Ethylene Propylene Rubber Peroxide cured, white Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Fede.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering E80B Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistan.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering E90K Ethylene Propylene Rubber General purpose, peroxide cured, Ethylene Propylene Terpolymer, 85-95 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM D2000/SAE J200 line call out M8CA910, A25, B35, C32, EA14, .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 910 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering C60M Chloroprene Rubber Chloroprene Rubber, 56-65 °IRHD. Formulated to meet British Standard BS2752 grade C60.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Kraiburg TPE THERMOLAST® K TC6HTT Transparent TPE, Outdoor Grade Transparent compounds with ideal UV resistance for outdoor applicationsSubstitute of silicone rubber or PVCNice design possibilities by coloring the compounds with a suitable polyolefin masterbatchT.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg R320 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg R408 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg E569 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg Emerson & Cuming Eccobond® A410-05P One-Component Thermally Conductive Epoxy Adhesive Emerson & Cuming A410-05P Eccobond® One-Component Thermally Conductive Epoxy AdhesiveHigh strength, aluminum filled, epoxy adhesive for bonding to most oily or other poorly prepared metal surfaces... |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Dow Corning 7 RELEASE COMPOUND Silicone-based compound, light consistencyInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | continuous (Cured condition) |
Dow BETAMATE™ 7205 Polyurethane Prepolymer BETAMATE™ 7205 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Dow Corning 111 VALVE LUBRICANT & SEALANT General purpose O-ring and valve lubricant. Provides a noncuring moisture barrier; high dielectric strength; moisture and ozone resistance; good thermal, oxidation and chemical stability; suitable .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Kraiburg TPE THERMOLAST® K TP8HPN Natural Extrusion TPE, Outdoor Grade
(Unverified Data**) Natural extrusion compound for outdoor useSubstitute for PVC-P and EPDMExcellent weldabilitySmooth surfaceGood UV and weathering resistanceTypical Applications: Seals and sealing profiles for window.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Kraiburg TPE THERMOLAST® K TP7HPN Natural Extrusion TPE, Outdoor Grade
(Unverified Data**) Natural extrusion compound for outdoor useSubstitute for PVC-P and EPDMExcellent weldabilitySmooth surfaceGood UV and weathering resistanceTypical Applications: Seals and sealing profiles for window.. |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® EX Damping Material, 0.20 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure without.. |