Indium Corp. Indalloy® 46L Ga-In-Sn-Zn Alloy for Mercury Replacement

Category Metal , Nonferrous Metal , Gallium Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 46L Ga-In-Sn-Zn Alloy for Mercury Replacement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 6.50 g/cc
0.235 lb/in³
Thermal Properties Metric English Comments
Melting Point 7.00 - 8.00 °C
44.6 - 46.4 °F
Solidus 7.00 °C
44.6 °F
Liquidus 8.00 °C
46.4 °F
Component Elements Properties Metric English Comments
Gallium, Ga 61 %
61 %
Indium, In 25 %
25 %
Tin, Sn 13 %
13 %
Zinc, Zn 1.0 %
1.0 %