Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Plasticizing Zone |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Processing Temperature | 80.0 - 150 °C | 176 - 302 °F | Average value: 118 °C Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2010829D2 Silver Ink Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be.. |
|||
Processing Temperature | 80.0 - 150 °C | 176 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin 75 NanoCoating Non-abrasive coating with extreme chemical resistance, also applicable for plastics substrates.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 60.0 - 150 °C | 140 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin 78 NanoCoating Transparent, scratch-resistant coating also for plastics with good resistance against dissolvents.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 80.0 - 150 °C | 176 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin 94 NanoCoating Non-abrasive coating with extreme chemical resistance, easy-to-clean, biocompatible, also for plastics.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 140 - 150 °C | 284 - 302 °F | Hardening Temperature |
Möller Medical PolySkin 81 NanoCoating Flexible, non-abrasive, decorative coating; easy-to-clean effect can be addedInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Lamination Adhesive |
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 130 - 150 °C | 266 - 302 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 100 - 150 °C | 212 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 100 - 150 °C | 212 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1566A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1712A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |