Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade Injection molding grade for very long flow paths, as well as thin-walled parts.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Tensile Strength, Ultimate | 62.0 - 100 MPa | 8990 - 14500 psi | Average value: 93.8 MPa Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM Data |
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2300 Phenolic, Granular, Compression Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® TR-5 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Adell YS-10 PC Alloy |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Chemlon 253 H Nylon 6, Impact Modified A medium viscosity impact modified, heat stabilized nylon 6 exhibiting improved toughness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Formax 609 Acetal, Medium Flow A 9 melt flow index, injection molding grade copolymer acetal.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled A mineral filled Nylon 66 providing superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 735 Nylon 6 Economy grade, impact modified Nylon 6 for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Formax 604 Acetal, Low Flow A 4 melt flow index copolymer acetal for extrusion or thick injection molding applications.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Formax 630 Acetal, High Flow A 30 melt flow index copolymer acetal for use in products requiring extreme demands on processing characteristics but only moderate demands on mechanical performance.Data provided by the manufacture.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D651 |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 62.0 - 83.0 MPa | 8990 - 12000 psi | Average value: 77.0 MPa Grade Count:10 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |