Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | ASTM D495 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | ASTM D495 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 180 sec | 180 sec | |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Arc Resistance | 180 sec | 180 sec | |
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Arc Resistance | 180 - 240 sec @Thickness 3.00 mm |
180 - 240 sec @Thickness 0.118 in |
(NC) |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
IDI Composites 46-12 Thermoset Polyester, Molding Highest strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer. |
|||
Arc Resistance | 180 sec | 180 sec | Post-cured, ASTM D495 |
Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-1. A superior replacement for epoxy-bonded mica in layer insulation applications. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | ASTM D495 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | UL 746A |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | UL 746A |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Arc Resistance | 180 - 240 sec | 180 - 240 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Arc Resistance | 180 sec | 180 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM 15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | 180 sec | 180 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TB120SG30 Impact Modified, 30% Glass Fiber Reinforced PA6, DAM 30% Glass Fiber reinforced, High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | IPC TM-650 2.5.1 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | D48/50; IPC TM-650 2.5.1B |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Arc Resistance | 180 sec | 180 sec | |
BCC Products BC 9040 T Silicone RTV Rubber BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high.. |
|||
Arc Resistance | >= 180 sec | >= 180 sec | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bak North America, Inc. |
|||
Arc Resistance | 180 sec | 180 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Arc Resistance | 180 sec | 180 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |