Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 12.0 GPa | 1740 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Modulus of Elasticity | 12.0 - 14.0 GPa | 1740 - 2030 ksi | Compression; ISO 527 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Modulus of Elasticity | 12.0 - 24.5 GPa | 1740 - 3550 ksi | Average value: 18.5 GPa Grade Count:13 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | ASTM D638 |
RTP Company RTP 282G TFE 15 HS Nylon 4/6 (PA 4/6) Carbon Fiber 15% - PTFE 15% - Heat Stable
&nbs Carbon Fiber 15% - PTFE 15% - Heat StableComments:Carbon FiberPTFE LubricatedHeat Stabilized(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigm.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1-8260 Polyamide 66, with glass fiber, thermally conductive modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Emergency running property.Coil formers, duty parts in plugs and switches, .. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1850/CF/15/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 20-8114 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 20-8244 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1105-0797 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Modulus of Elasticity | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |