Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Dielectric Strength | 24.0 - 25.0 kV/mm | 610 - 635 kV/in | Average value: 24.3 kV/mm Grade Count:3 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Asia Pacific) Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.60 mm |
610 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.60 mm |
610 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 3.20 mm |
610 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® QC220N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 35% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant, Heat Stabilized and High Temperature Strength UL .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics Duranex® 313RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 64 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 85 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 3.17 mm |
610 kV/in @Thickness 0.125 in |
50% R.H.; ASTM D149 |
Celanese Celanex® 7700 Polyester (PBT), 35% Glass/Mineral Flame retardant and low warpInformation provided by Celanese Corporation. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 5.00 mm |
610 kV/in @Thickness 0.197 in |
IEC 60243-1 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |