Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 80.0 - 150 °C | 176 - 302 °F | Average value: 118 °C Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | Cavity temperature |
Celanese ZENITE 6140L LCP, 40% Glass Reinforced
(Unverified Data**) Zenite® 6140L is a 40% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.40% glass rei.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2010829D2 Silver Ink Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be.. |
|||
Processing Temperature | 60.0 - 150 °C | 140 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin 78 NanoCoating Transparent, scratch-resistant coating also for plastics with good resistance against dissolvents.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 140 - 150 °C | 284 - 302 °F | Hardening Temperature |
Möller Medical PolySkin 102 M NanoCoating Decorative, thermally stable coating with "metallic look," easy-to-clean effect can be added.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 140 - 150 °C | 284 - 302 °F | Hardening Temperature |
Möller Medical PolySkin 81 NanoCoating Flexible, non-abrasive, decorative coating; easy-to-clean effect can be addedInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2010515D4 Silver Ink Silver Ink C2010515D4 is designed as an internal electrode ink for LTCC applications. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the mark.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1260 A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 130 - 150 °C | 266 - 302 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 100 - 150 °C | 212 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1566A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | cavity |
Celanese ZENITE 6140L LCP, 40% Glass Reinforced Zenite« 6140L is a 40% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.Information p.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | cavity |
Celanese ZENITE 6244L LCP, 40% Mineral / Glass Reinforced Zenite 6244L is a lubricated, 40% glass fiber and mineral reinforced liqud crystal polymer resin. It is well suited for use in the automotive, electrical/electronic, telecommunications, and aerospa.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | cavity |
Celanese ZENITE 7140X LCP, 40% Glass Reinforced Zenite 7140X is a 40% glass reinforced liquid crystal polymer resin with improved weldline strength, low post soldering warpage and a heat deflection temperature of 298C."Information provided by Cel.. |
|||
Processing Temperature | 100 - 150 °C | 212 - 302 °F | cavity |
Celanese THERMX LED 0201S PCT, 38% Specialty Thermx LED 0201S is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low mois.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | cavity |
Celanese ZENITE 6330 LCP, 30% Mineral Reinforced Zenite« 6330 is a 30% mineral reinforced liquid crystal polymer for injection molding. It has excellent impact resistance, excellent heat deflection temperature and and is well suited for all kinds.. |
|||
Processing Temperature | 40.0 - 150 °C | 104 - 302 °F | cavity |
Celanese ZENITE ZE16401 LCP, 30% Specialty Zenite« ZE16401 is a 30% mineral reinforced and Teflon« PTFE powder filled liquid crystal polymer for injection molding. and It is well suited for low wear / low friction applications.Information .. |
|||
Processing Temperature | 100 - 150 °C | 212 - 302 °F | Cavity temperature |
Celanese Thermx® LED 0201S PCT, 38% Specialty
(Unverified Data**) Thermx LED 0201S is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low mois.. |