Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Menzolit
Trade Name Menzolit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Typical applications are housings and covers in the electrical industry. Usually it is used for functional parts that don't require a high fire retardancy.Information Provided by Menzolit
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.0 MPa

@Temperature 22.0 °C
5080 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Tensile Strength, Yield 35.0 MPa

@Temperature 22.0 °C
5080 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Modulus of Elasticity 13.0 GPa
1890 ksi
25mm flat samples, compression moulded; ISO 527-4
Flexural Strength 120 MPa

@Temperature 22.0 °C
17400 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa

@Temperature 22.0 °C
1450 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
0.30
Shear Modulus 5.00 GPa
725 ksi
in plane
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 130 °C
>= 266 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 170 °C
338 °F
ISO 11357-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 22 %
22 %
ISO 4589-2
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 150 °C
275 - 302 °F
Injection moulding, matched metal die
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved