Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 13.0 - 15.0 GPa | 1890 - 2180 ksi | Injection; ISO 527 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | ASTM D638 |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Modulus of Elasticity | 13.0 - 22.5 GPa | 1890 - 3260 ksi | Average value: 18.0 GPa Grade Count:12 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour... |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 50-7644 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f.. |
|||
Modulus of Elasticity | 13.0 GPa | 1890 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Modulus of Elasticity | 13.0 GPa @Thickness >=1.50 mm |
1890 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc.. |