Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.5%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 70.5% F grade terpolymer with best pe.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | True Density |
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
(discontinued **) QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber
(discontinued **) Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
IDI Composites C-103 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4201 General Application Gasketing Synthetic FiberNitrile BinderExcellent Resistance to Oil & SolventsGood Anti-Stick PropertiesExcellent OEM MaterialInformation provided by Thermoseal Inc. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-181 Compression Molded PPEK Compound, EWS Filled and Carbon Fiber Reinforced Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.90 - 2.20 g/cc | 0.0686 - 0.0795 lb/in³ | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion.. |
|||
Density | 1.90 - 2.10 g/cc | 0.0686 - 0.0759 lb/in³ | Molded |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C). |
|||
Density | 1.90 - 1.95 g/cc | 0.0686 - 0.0704 lb/in³ | |
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC
(discontinued **) QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |