Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.90 g/cc | 0.0686 lb/in³ | |
3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.5%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 70.5% F grade terpolymer with best pe.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | True Density |
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH FR15030 XNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L V 9113-2 PPS, 60% Glass Fiber
(discontinued **) Glass Fiber Grade with Highest Mechanical Strength and Stiffness. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Housings for Shock Absorbers and Spring ElementsProce.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral
(discontinued **) Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (M.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
IDI Composites W-102 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
IDI Composites W-103 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y H-VAC 25/9 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
TriStar CJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4408 Metal Reinforced Gasketing Synthetic FiberNitrile BinderHigh Temperature & StressFluctuating Temperatures & PressuresVibrationLow Carbon Steel Woven Mesh InsertInformation provided by Thermoseal Inc. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
Goodfellow E-glass/Epoxy Composite Boro-silicate glass/EpoxyInformation provided by Goodfellow. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
Cotronics Duralco™ 4525 Electrically Resistant, Room Temperature Curing Epoxy High bond strength, high thermal stability, low moisture absorption, low shrinkage and excellent chemical, electrical, and radiation resistance.Chemical Resistance: resistant to hydrochloric, phosph.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | |
Cytec Thornel® P-25 4K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield.. |
|||
Density | 1.90 - 2.20 g/cc | 0.0686 - 0.0795 lb/in³ | |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only) Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Inj.. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® S-206 PPS Resin Glass fiber reinforced and mineral filledInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.90 - 2.10 g/cc | 0.0686 - 0.0759 lb/in³ | Molded |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Density | 1.90 g/cc | 0.0686 lb/in³ | ASTM D792 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | |
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |