Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant , Polystyrene, Impact Modified
Manufacturer LTL Color Compounds
Trade Name ColorFast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
0.125; ASTM D955
Melt Flow 6.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 61
61
ASTM D785
Tensile Strength at Break 24.8 MPa
3600 psi
2.0 in/min; ASTM D638
Tensile Strength, Yield 24.1 MPa
3500 psi
2.0 in/min; ASTM D638
Elongation at Break 35 %
35 %
2.0 in/min; ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
2.0 in/min; ASTM D790
Izod Impact, Notched 0.961 J/cm

@Temperature 22.8 °C
1.80 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
Unannealed (0.250"); ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Rear Barrel Temperature 171 - 199 °C
340 - 390 °F
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Front Barrel Temperature 218 - 254 °C
425 - 490 °F
Nozzle Temperature 204 - 232 °C
400 - 450 °F
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 10.0 - 71.1 °C
50.0 - 160 °F
Drying Temperature 71.1 °C
160 °F
Dry Time 2 - 4 hour
2 - 4 hour
nominal; maximum drying time of 8 hours
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Shot Size 40 - 60 %
40 - 60 %
Vent Depth 0.00254 - 0.00762 cm
0.00100 - 0.00300 in
Screw Speed 40 - 70 rpm
40 - 70 rpm