Polymer Property : Melt Temperature = 238 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 227 - 238 °C
440 - 460 °F
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced
Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Melt Temperature 216 - 238 °C
421 - 460 °F
PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 216 - 238 °C
420 - 460 °F
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Melt Temperature 216 - 238 °C
420 - 460 °F
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 600 FR AB Acrylonitrile Butadiene Styrene (ABS), Medium Impact - Flame Retardant - UL94 V-0
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 600 TFE 20 Acrylonitrile Butadiene Styrene (ABS), PTFE Lubricated
Melt Temperature 182 - 238 °C
360 - 460 °F
RTP Company RTP 6001-70A Z Specialty Thermoplastic Elastomer, FDA Compliant Ingredients
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-55A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6003-75A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 601 FR A Acrylonitrile Butadiene Styrene (ABS); Glass Fiber - Flame Retardant
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-40A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-40A Z Specialty Thermoplastic Elastomer
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company RTP 6042-60A Specialty Thermoplastic Elastomer, PC/ABS Bondable
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 681 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - Flame Retardant
The RTP 680 FR Series offers a good combination of physical properties, stiffness, ignition resistance and the ability to be fabricated to close dimensional tolerances.
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 682 HEC FR Acrylonitrile Butadiene Styrene (ABS), Nickel-Coated Carbon Fiber - Flame Retardant - Electrically Conductive - EMI/RFI/ESD Protection
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company RTP 683 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB
The RTP 680 HB are carbon fiber reinforced ABS. These materials offer a good combination of physical properties, stiffness and the ability to be fabricated to close dimensional tolerances.
Melt Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring..
Melt Temperature 216 - 238 °C
421 - 460 °F
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app..
Melt Temperature 221 - 238 °C
430 - 460 °F
Molding
PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company ESD C 600 Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Electrically Conductive
Melt Temperature 204 - 238 °C
400 - 460 °F
RTP Company PermaStat® 1000 Polybutylene Terephthalate (PBT), Permanently Anti-static - ESD Protection
Melt Temperature 199 - 238 °C
390 - 460 °F
RTP Company PermaStat® 600 Nat/Clear Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static - Transparent Grade
Melt Temperature 199 - 238 °C
390 - 460 °F
RTP Company PermaStat® 600 UV Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static - UV Stabilized
Melt Temperature 210 - 238 °C
410 - 460 °F
RTP Company RTP 1500.5-50D Polyether-Ester Block Copolymer (TEEE / COPE), Glass Fiber
Melt Temperature 227 - 238 °C
440 - 460 °F
CTC X-PRO TF 2104 GP Recycled Polypropylene Homopolymer, 20% Talc Filled
X-PRO TF 2104 GP is a 20% talc reinforced polypropylene homopolymer made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.D..
Melt Temperature 221 - 238 °C
430 - 460 °F
Celanese Riteflex® 655 Thermoplastic Polyester Elastomer (TPE)
Information provided by Celanese Corporation.
Melt Temperature 216 - 238 °C
421 - 460 °F
LookPolymers® D4302 Thermally Conductive Polybutylene Terephthalate
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Melt Temperature 193 - 238 °C
380 - 460 °F
RTP Company PermaStat® 203 A Nylon 6 (PA), Glass Fiber - ESD Protection - Permanently Static Dissipative