Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 71.1 - 76.7 °C | 160 - 170 °F | |
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 76.7 °C | 160 - 170 °F | |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne Edgetek® NN-30GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | 2 hrs |
PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.0 - 82.0 °C | 160 - 180 °F | |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.1 - 82.2 °C @Time 7200 sec |
160 - 180 °F @Time 2.00 hour |
|
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 °C | 160 °F | Drying not normally required |
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 71.1 °C | 160 °F | ASTM D648 |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Drying Temperature | 71.1 °C | 160 °F | |
Hexcel® Redux® 108 Surface Pretreatment Protection Solution The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
Hexcel® Redux® 119 Surface Pretreatment Protection Solution The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Ecomass® 720ZC85 Stainless Steel Filled ABS High Specific GravityStainless Steel Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers |
|||
Drying Temperature | 71.1 - 85.0 °C | 160 - 185 °F | or lower with overnight predrying |
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-10GF-10KV/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 71.1 °C | 160 °F | |
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc. |