Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3340-65A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Mold Temperature | 10.0 - 35.0 °C | 50.0 - 95.0 °F | Injection Molding |
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 10.0 - 35.0 °C | 50.0 - 95.0 °F | Injection Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 10.0 - 40.0 °C | 50.0 - 104 °F | |
Lucobit Lucofin® 1411 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Mold Temperature | 10.0 - 40.0 °C | 50.0 - 104 °F | |
Lucobit Lucofin® 1415 Polyolefin TPO Granules, Signal White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene Available in standard black.Information provided by MBA Polymers. |
|||
Mold Temperature | 10.0 - 60.0 °C | 50.0 - 140 °F | Injection Molding |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Mold Temperature | 10.0 - 60.0 °C | 50.0 - 140 °F | ISO 294 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Mold Temperature | 10.0 - 65.6 °C | 50.0 - 150 °F | Injection Molding |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
Mold Temperature | 10.0 - 65.6 °C | 50.0 - 150 °F | Injection Molding |
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BC650MO Polypropylene Copolymer BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HD120MO Polypropylene HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf.. |
|||
Mold Temperature | 10.0 - 40.0 °C | 50.0 - 104 °F | |
Borealis MG9641S Polyethylene MG9641S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Mold Temperature | 10.0 - 79.4 °C | 50.0 - 175 °F | |
RTP Company RTP 2800 B-45A Z Thermoplastic Polyolefin Elastomer (TEO) FDA Compliant Ingredients |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | actual surface temp |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Mold Temperature | 10.0 - 65.6 °C | 50.0 - 150 °F | Injection Molding |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Mold Temperature | 10.0 - 35.0 °C | 50.0 - 95.0 °F | Injection Molding |
LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Mold Temperature | 10.0 - 40.0 °C | 50.0 - 104 °F | |
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESC.. |
|||
Mold Temperature | 10.0 - 51.7 °C | 50.0 - 125 °F | Processing |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |