Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM 792 |
Multibase Nylex™ 4032 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | 23/23°C; ASTM D792 |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Polymax® Maxelast® P1770 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D 792 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 1088-10 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **)&l |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | |
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Specific Gravity | 1.15 - 1.21 g/cc | 1.15 - 1.21 g/cc | ASTM D 792 |
Karina Polar Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.15 g/cc @Temperature 22.8 °C |
1.15 g/cc @Temperature 73.0 °F |
ASTM D792 |
Spartech PP7130 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7345-1000 TPE Product Description: StarFlex P 7345-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 90-A472R-55-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Supreme Petrochem SP 554 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Lubrizol Estane® ALR PC85A Thermoplastic Polyurethane Type: Estane® ALR PC85A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | PVC (70)/CP80AS2(30) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Colorite Polymers CS1515GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | Mixed; TM R050-16 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Specific Gravity | 1.15 - 1.21 g/cc | 1.15 - 1.21 g/cc | ASTM D 792 |
Karina 66/200-DA-IS-SI Clear PVC Compound PVC compound recommended for extrusion of butcher's shop curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |