Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® M-2450 Polypropylene Copolymer Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 5002 Polypropylene Copolymer X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1020 GP is a 20% talc reinforced polypropylene homopolymer. It has applications in general purpose industrial, automotive, consumer, and construction.Data provided by Composite Technologies.. |
|||
Middle Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled X-PRO TF 1113 HP is a 13% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |